It is core type and manufactured from 0.30, 0.25 and 0.23 mm thick M5, M4 and M3 silicon alloy sheets with oriented crystals. 45 degree inclined cut sheets are used in the transition areas of the magnetic circuit. All sheets used in the magnetic circuit are cut by CNC controlled cutting machine, stacked and arranged to form the magnetic circuit. Magnetic circuit cutting and arrangement is done with a method called step-lab which minimizes iron losses. The core is arranged with cross and longitudinal step-lab applications.
Our leg and yoke sections are equal, multi-stage and theoretically round in section.
Noise levels are minimized by compressing the core sheets with steel studs passing through the U profile and yoke insulating pipes.